Hi there,

I’m wondering if I could get some advice on why my prints are always failing at 0.2mm layer height

Attached is a pic, the first layers are perfect but as it gets to layer 3-4 I the print does not stick to the previous layers!

Printing at 0.1mm is absolutely perfect, first layer is perfect etc (in my opinion)

Just wanted to have the option for a 0.2mm height so the prints don’t take as long.

Printer is Kingroon KP3S Pro V2 with Klipper Slicer is OrcaSlicer

I can share configs from either if needed, or more close up pics.

Cheers

11

You're viewing a single thread.

11 comments
  • Would bumping up your printing temp do anything?

    • It's already running 225 for PLA since it's a hardened steel nozzle, but I tried it on 230 with the same result